gEDA-user: fun/easy BGA part
DJ Delorie
dj at delorie.com
Sat Dec 16 14:28:05 EST 2006
> Yes, exactly. The idea is that with uniform heating, the balls
> should all melt the same way at the same time.
Hopefully, you can see the whole part settle once the final ball
melts, too. From what I've read, the problem isn't the melting, it's
the quality of the connection. For production, x-ray inspection is
required. For home use, I suspect either good fluxing or a little
solder paste is going to be key to getting a good reflow.